I have one very similar to the pexto. It leaves a slight dimple at the 
center and a very slight burr. All in all I use it if I need 3 or more 
circles. Fewer and I am good to go with a scribe and a pair of aviation 
snips. Just cut squares 5.25 or so center the scribe at 5 and cut it out.

Mike Graf

On 9/6/2012 7:20 AM, Andrew Vida wrote:
> Have not tried this, if I understand the tool to which you refer which
> has a reciprocating punch that nibbles its way along.  That would seem
> painful, particularly if you need any accuracy.
>
> The fastest and best way to do this, beyond having a nice large water
> jet rig would be a circle shear.  I have a small one that needs to be
> set up... as do so many other things.
>
> A quick peek on ebay shows no hand shears available, only powered ones
> and they are costly.  But one of those would be your best bet.  Cut a 5"
> circle perfectly in under 30 seconds.
>
> Price may be worth it if you have a lot to cut.  There is this one:
>
> http://www.ebay.com/itm/Libert-Shear-Nibbler-Circle-Shear-Hi-Speed-3-phase-motor-/270910652486?pt=LH_DefaultDomain_0&hash=item3f13888046
>
> and this:
> http://www.ebay.com/itm/PEXTO-CIRCLE-SHEAR-/290713684998?pt=LH_DefaultDomain_0&hash=item43afe2cc06
>
> Or this - perhaps you can make one for yourself:
>
> http://www.ebay.com/itm/Greenlee-No-740-Sheet-Metal-Hole-Circle-Cutter-Machinist-Electrician-Heating-use-/190723179163?pt=LH_DefaultDomain_0&hash=item2c67fcc29b
>
>
>
> On 9/5/2012 12:05 PM, Ron Childers wrote:
>>
>>
>> Has anyone tried a pneumatic panel cutter (like a muffler cutter) to cut
>> 5" circles in brass sheet?
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoworks.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>


More information about the TheForge mailing list