On 11/6/2012 3:25 PM, James Binnion wrote:
> It is intended to limit electrolytic corrosion of the connection. It will not keep the contacts from making electrical connection but will prevent water and road gunge (technical term) from creating a short circuit or causing the contacts to be eaten up by electrolytic corrosion.
>
> Electrically conductive grease OTOH is for moving or rotating electrical connections to prevent/reduce arcing during motion.
>
>
>