[TheForge] Anvil Repair - 7018 Rod use
dan tull
dantull at numail.org
Wed Mar 14 14:19:02 EDT 2012
Why are you using 7018?
It's a low Hydrogen rod used by pipe and tank welders that have to have
x-ray/magnaflux. Soon as you open the can, it starts absorbing and ruining.
That's why they throw away partial boxes at the end of the day. The 70XX is
stronger(harder??) than 60XX only in tension.Anvil pounding is compression.
Why don't you look at MG750 rod. It was created for repair for the ROCK
CRUSHING industry.
HIGHEST IMPACT rod. Not abrasaweld that just grinds off hard. Extra benefit:
NO pre-post heating. DUH! Plus it is excellent for welding dis-similar
carbon steels(as in mild hardy tangs to high carbon tools). Lay a base w/ a
6011 "plunge" rod to tie face to body, and lay MG750 over. Hint : watch out
for popping slag as your weld cools.
Expensive? $2/stick, so split a box w/ another smith.
I have patched up many anvils in 24 yrs, and have not had a failure w/ this
rod.
And I don't own stock in MG.
----- Original Message -----
From: <Vincent_Nakovics at nps.gov>
To: <theforge at mailman.qth.net>
Sent: Wednesday, March 14, 2012 12:41 PM
Subject: Re: [TheForge] Anvil Repair - 7018 Rod use
> Thanks for the input Jerry,
>
> I was worried that I had it wrong. We have repaired 2 anvils using the
> preheat and 7018 method now. Last night was the first time I used my anvil
> that I repaired just last week. after I was done making my piece I couldn
> not resist tapping the edges that we repaired with my 3lb hammer. They
> weren't full smashing blows, but you wouldn't want your fingers there. The
> repair spots did not dent. I was happily impressed! The NJBA I believe did
> a bunch of repairs and that's where I got all my info from. (I could be
> wrong about the org, I just jotted down the pertinent stuff a while
> back.).
> So far it has worked for the two that we have done. Preheat anvil, use
> 7018
> Rod. grind, sand, walla!
>
> Vince
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list