On 12/22/2012 4:45 PM, Peter Fels & Phoebe Palmer wrote:
> Bob:
> What's the triangle of welding?
> Stellite too! Wow!

Ever try to forge real stellite?  I crumbles.  There are many so-called 
"stellites", but the real deal, the original material, has no iron in it 
as I recall, though do not quote me on that.  I once attempted to forge 
a stellite bit and it did not go well at all.