[TheForge] black pipe
Larry Brown
lp.brown at verizon.net
Thu Dec 20 22:18:44 EST 2012
Acetylene torch with O2 rich flame or trigger pulled a bit, wire brush the
ash off. Use ventilation or do outside, not usually noxious but can be
smokey. Cant say what is on the chinese stuff, just assume it's toxic
L Brown
At 06:44 PM 12/20/2012 -0600, you wrote:
>It's coated with a varnish material. Try paint stripper.
>We never used to worry about removing it when it was installed. It seems
>the painters could just clean it with a rag and paint right over it. But
>most of the time after installation it was covered with pipe insulation...
>never had to look at it again unless we had to tie into it.
>
>Paul
>
>
>On 12/20/2012 06:15 PM, Mark and Sylvia Mondloch wrote:
>>Has anyone found an easy way to get the stuff they put on black pipe off.
>>I have used sandblasting but there has got to be a better way.
>>
>>Mark and Sylvia Mondloch
>>Silver Creek Pottery & Forge
>>mondloch at silvercreekpottery.com
>>www.silvercreekpottery.com
More information about the TheForge