I have weld up some blades with my mig and a jig that i made you but it 
dosen.t do a graet job  need to by a blade welder. jim o.:
> A Cut Above...the abrasive outfit used to sell blades at a reasonable price, most probably still do.
> Silver soldering the blades is a little fussy, but not all that difficult.
> Have to grind opposed tapers at the ends and clamp the overlapping ends up true..put some flux and bits of solder between the tapers and gently heat from below. Then file the excess and any little bulge down flat again.
> An angle iron jig with a gap in the center for the joint is easy to fake .
>
> On Sep 6, 2011, at 11:50 AM, Jerry Frost wrote:
>
>> 92 1/2", is that x 3/4' or x1/2"? I have a horizontal vertical Jet and the
>> outfit I bought it from doesn't carry blades! Makes me want to scream,
>> they'll GET them but last time they sent the ones THEY determined I needed,
>> not what I ordered. I refused delivery on the wrong ones and they're a
>> serious PITA about blades now. The other down side is finding them online I
>> admit I haven't looked very hard but it shouldn't take but one search to
>> find a bunch of suppliers.
>>
>> Makes me want to buy a 3/4" band welder and make my own. Grrrrr.
>>
>> Sorry for the rant, Jer
>> ----- Original Message -----
>> From: "JAMES OESTREICH"<jimoest at charter.net>
>> To:<theforge at qth.net>
>> Sent: Tuesday, September 06, 2011 1:04 AM
>> Subject: [TheForge] saw blade
>>
>>
>>> don't post very often but need a source of band saw blade for cutting
>>> metal 92 1/2  long at a good price thank you all  jim o.
>>> ______________________________________________________________
>>> TheForge mailing list
>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>> Help: http://mailman.qth.net/mmfaq.htm
>>> Post: mailto:TheForge at mailman.qth.net
>>>
>>> TheForge mail list group photo site is
>>> http://www.photoworks.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> Password: anvil
>>>
>>> This list hosted by: http://www.qsl.net
>>> Please help support this email list: http://www.qsl.net/donate.html
>>>
>>>
>>> -----
>>> No virus found in this message.
>>> Checked by AVG - www.avg.com
>>> Version: 10.0.1392 / Virus Database: 1520/3880 - Release Date: 09/06/11
>>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoworks.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>



More information about the TheForge mailing list