sorry, but aluminum is used in steel alloys, in tiny percentages. good deep drawing steel is usually AK- "aluminum killed".

ries


On Nov 27, 2011, at 5:34 PM, Andy Gladish wrote:

> I think I need to call BS on something that Hodges said on the newest
> Bones- "...an alloy of aluminum and steel..."
> There IS no such thing, yes no?
> Andy G
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html

Ries Niemi
Industrial Artist
www.riesniemi.com





More information about the TheForge mailing list