[TheForge] Metallurgy and Powder Coating
peter fels
artgawk at thegrid.net
Tue May 31 12:48:43 EDT 2011
Good to know, thanks Andy.
On May 31, 2011, at 5:59 AM, Andrew Vida wrote:
> You NEVER ever powder coat aluminum SCUBA tanks for those precise
> reasons. I have heard several third-hand accounts of this happening.
> Ignorance can be very dangerous.
>
> Ron Childers wrote:
>> Craig,
>>
>> A friend of mine, a famous cave diver, had a fancy paint job done on his
>> aluminum scuba cylinders and it was baked on. The heat apparently
>> weakened the metal to the extent it exploded during the first fill
>> causing serious injury and the schrapnal wreaked havoc with the dive
>> shop. I don't know the baking heat or the alloy of the cylinder, but it
>> did weaken it. You might consider anodizing if you want a pretty color.
>> Ron C
>>
>> -----Original Message-----
>> From: theforge-bounces at mailman.qth.net
>> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Craig Schaefer
>> Sent: Friday, May 27, 2011 11:41 PM
>> To: Blacksmithing List Sponsored by ABANA
>> Subject: [TheForge] Metallurgy and Powder Coating
>>
>> I have some aluminum alloy motorcycle brake calipers and wheels that I'd
>>
>> like to powder coat. Would I weaken the aluminum by the heating
>> process to
>> the 400-500 degree range?
>> I know others offer the service, but that doesn't mean it's a good idea.
>>
>> CraigS
>> Gresham, OR
>>
>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoworks.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoworks.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list