Jim Poulimas poulmas at gmail.com
Tue May 31 09:09:27 EDT 2011


Craig,
I wouldn't heat any of the components for your motorcycle. Whatever the
manufacturer ships out is what you should use - unless designed otherwise.
Especially with motorcycles.
Jim

On Tue, May 31, 2011 at 7:47 AM, Ron Childers <ron at munlaw.net> wrote:

> Craig,
>
> A friend of mine, a famous cave diver, had a fancy paint job done on his
> aluminum scuba cylinders and it was baked on. The heat apparently
> weakened the metal to the extent it exploded during the first fill
> causing serious injury and the schrapnal wreaked havoc with the dive
> shop. I don't know the baking heat or the alloy of the cylinder, but it
> did weaken it. You might consider anodizing if you want a pretty color.
> Ron C
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Craig Schaefer
> Sent: Friday, May 27, 2011 11:41 PM
> To: Blacksmithing List Sponsored by ABANA
> Subject: [TheForge] Metallurgy and Powder Coating
>
> I have some aluminum alloy motorcycle brake calipers and wheels that I'd
>
> like to powder coat.   Would I weaken the aluminum by the heating
> process to
> the 400-500 degree range?
> I know others offer the service, but that doesn't mean it's a good idea.
>
> CraigS
> Gresham, OR
>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>



-- 
*poulimasiron.com
203 887 7326
*


More information about the TheForge mailing list