[TheForge] Proper disposal of hazmat
wmullett at bright.net
wmullett at bright.net
Mon May 23 09:54:06 EDT 2011
And people complain about governmental regulation.
---- Original message ----
>Date: Sat, 21 May 2011 09:03:22 -0500
>From: theforge-bounces at mailman.qth.net (on behalf of Cindy and James <jallcorn at suddenlink.net>)
>Subject: [TheForge] Proper disposal of hazmat
>To: theforge at mailman.qth.net
>
>My wife's cousin is a truck driver for a co. in GA, hauling haz waste,
>usually used sulfuric acid used in industrial steel pickling. They haul
>it to Louisiana and dump it in a swamp. So much for proper recycling. JA
>
>On 5/20/2011 8:02 AM, theforge-request at mailman.qth.net wrote:
>> Send TheForge mailing list submissions to
>> theforge at mailman.qth.net
>>
>> To subscribe or unsubscribe via the World Wide Web, visit
>> http://mailman.qth.net/mailman/listinfo/theforge
>> or, via email, send a message with subject or body 'help' to
>> theforge-request at mailman.qth.net
>>
>> You can reach the person managing the list at
>> theforge-owner at mailman.qth.net
>>
>> When replying, please edit your Subject line so it is more specific
>> than "Re: Contents of TheForge digest..."
>>
>>
>> Today's Topics:
>>
>> 1. Re: electrolysis (Ron Childers)
>> 2. Re: electrolysis (woolley)
>> 3. Re: electrolysis (Ron Childers)
>> 4. Re: electrolysis (Bruce Freeman)
>> 5. Re: electrolysis (Geoff Nelson)
>> 6. Re: electrolysis (Ron Childers)
>> 7. Re: electrolysis (Paul Sperbeck)
>> 8. Re: electrolysis (Ron Childers)
>>
>>
>> _______________________________________________http://mailman.qth.net/mailman/listinfo/theforge
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>>
>>
>______________________________________________________________
>TheForge mailing list
>Home: http://mailman.qth.net/mailman/listinfo/theforge
>Help: http://mailman.qth.net/mmfaq.htm
>Post: mailto:TheForge at mailman.qth.net
>
>TheForge mail list group photo site is
>http://www.photoworks.com
>Login: blacksmithblacksmith at hotmail.com
>Password: anvil
>
>This list hosted by: http://www.qsl.net
>Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list