...but that doesn't account for heat of fusion, which, if high enough,
can retard melting considerably.

On Wed, Jun 15, 2011 at 7:45 AM, Bruce Freeman <freemab222 at gmail.com> wrote:
> Wikipedeia is a good source:
> http://en.wikipedia.org/wiki/Zirconia
> MP ~2700F.  Doesn't sound impressive, but
>
> On Wed, Jun 15, 2011 at 1:22 AM, peter fels <artgawk at thegrid.net> wrote:
>> I'd forgotten about that stuff Jerry...wonder how high it will go?
>> I recall some of the chrome oxides are pretty high temp too.
>>
>> So,,Graphene, zirconium oxide and cornstarch?
>>
>> Graphene
>> On Jun 14, 2011, at 6:09 PM, Jerry Frost wrote:
>>
>>> Zirconium oxide Pete. Though it's a ceramic not a salt but it has a REALLY
>>> high melting temp and a high IR albedo. I coat my forges with it by the
>>> brand name ITC-100. It's darned flux resistant and I've had molten steel
>>> laying on it to no ill effect.
>>>
>>> Zirconium is the first thing I thought of upon reading the article.
>>>
>>> Jer
>>> ----- Original Message -----
>>> From: "peter fels" <artgawk at thegrid.net>
>>> To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
>>> Sent: Tuesday, June 14, 2011 2:11 AM
>>> Subject: Re: [TheForge] plastic forge? OT:
>>>
>>>
>>>>
>>>> On Jun 13, 2011, at 12:41 PM, Bruce Freeman wrote:
>>>>
>>>>> Of course!
>>>>>
>>>>> Oxygen is a gas at room temperature and pressure.  Silicone is a solid
>>>>> melting at about 2500*F.  Silicon dioxide (aka quartz or silica) is a
>>>>> solid melting at about 3000*F - a covalent compound of the three
>>>>> atoms.  And there are much more dramatic examples than this.
>>>>>
>>>>> Sodium is a low-melting metal (~208*F).  Chlorine is a gas at room
>>>>> temperature.  Sodium chloride is a solid salt melting around 1500*F.
>>>>>
>>>>> The difference is that metals like tin and lead, typically don't
>>>>> combine chemically -- forming new molecules or salts -- whereas oxides
>>>>> like quartz are distinctly new entities, molecules.  In some respects,
>>>>> a molecule is like an extended atom -- the electrons are shared
>>>>> between the nuclei.  Salts are rather the opposite -- the electrons
>>>>> are not shared, but rather passed completely from one to the other,
>>>>> resulting in an electric charge that keeps the ions together (unless
>>>>> stabilized by a polar solvent, like water).  Hence, property changes
>>>>> can be pretty dramatic.
>>>>
>>>> Then is there a handy, refractory  salt of high melting temperature metals
>>>> or elements?
>>>>>
>>>>> A couple more thoughts:
>>>>>
>>>>> A material can "resist" energy (i.e., photons) by reflecting it or
>>>>> transmitting it (i.e., being transparent to it).  In addition to
>>>>> reflecting energy, a material can fluoresce -- absorb photons of one
>>>>> energy level and emit those of a lower energy level.  All these
>>>>> mechanisms could account for a substance surviving in the presence of
>>>>> intense energy.  Not all of them are useful for all purposes.
>>>>>
>>>>> On Mon, Jun 13, 2011 at 1:43 PM, peter fels <artgawk at thegrid.net> wrote:
>>>>>> In the interesting model you propose, the functional limit is the
>>>>>> temperature at which the "glass" breaks down...even if the carbon core
>>>>>> were to remain stable up to then.
>>>>>> The magical plastic alleges to exceed the limits of it's constituent
>>>>>> elements incredibly ( literally).
>>>>>> In metal alloys, a combination of elements tends to lower the melting
>>>>>> temperature.
>>>>>> Are there high temperature compounds where the opposite is dramatically
>>>>>> true?
>>>>>>
>>>>>> On Jun 13, 2011, at 4:40 AM, Bruce Freeman wrote:
>>>>>>
>>>>>>> Rather than wonder about this magical substance that notably has never
>>>>>>> been commercialized, why not brainstorm to find something or some
>>>>>>> things that fill some of those functions.
>>>>>>>
>>>>>>> There are, for example, a number of ways to resist heat.  Most
>>>>>>> refractories (graphite being a notable exception) that resist heat by
>>>>>>> virtue of high melting point and being oxides (impossible to further
>>>>>>> oxidize).  Others are ablative -- sacrificial.  Graphite almost falls
>>>>>>> into the last category, or maybe does.
>>>>>>>
>>>>>>> Suppose you try to use bituminous coal as a refractory.  Get it hot
>>>>>>> enough and it expands into breeze (coke).  It fails at that point
>>>>>>> because it starts to burn, but what if it were somehow protected from
>>>>>>> burning by a refractory "glass" layer.  Hence, composite something
>>>>>>> like bituminous coal with some sort of high-temperature
>>>>>>> oxidation-resistant substance.  What's neat about this is that the
>>>>>>> breeze would then act as an insulator, protecting what's beneath.
>>>>>>>
>>>>>>> What you want to do is to form your "clinker" right on the surface of
>>>>>>> the breeze.   So, this all gives rise to the question of why
>>>>>>> bituminous coal does not already act as a refractory.  I suspect that
>>>>>>> probably relates to properties of the breeze vs. the "glass".  Maybe
>>>>>>> the glass won't "wet" the carbon?  Maybe the continual degassing of
>>>>>>> the coal breaks the glass layer, making it ineffective as a "flux"?
>>>>>>> Maybe the glass sits on the outside of the breeze only, leaving the
>>>>>>> open "gas bubbles" exposed to the air blast?  Solve this problem and
>>>>>>> you might develop.  Even light microscopy could help determine the
>>>>>>> facts, and scanning electron microscopy would probably solve it in no
>>>>>>> time.
>>>>>>>
>>>>>>> Of course, graphite is mainly of interest because of it's high melting
>>>>>>> point.  Perhaps the equivalent behavior could be obtained using more
>>>>>>> standard ceramics.  But the "plastic" nature of our hypothetical
>>>>>>> material is now conceivably a problem.  How does one form a ceramic in
>>>>>>> a plastic manner?  Well, cement comes to mind -- castable or rammable
>>>>>>> refractories.
>>>>>>>
>>>>>>> All just brainstorming.
>>>>>>>
>>>>>>> On Mon, Jun 13, 2011 at 3:11 AM, peter fels <artgawk at thegrid.net>
>>>>>>> wrote:
>>>>>>>> It's hard to refrain from thinking of different applications for
>>>>>>>> it....
>>>>>>>> sorta like relations with  a harbor Fright catalogue when i was
>>>>>>>> poorer.
>>>>>>>>
>>>>>>>>
>>>>>>>> On Jun 12, 2011, at 3:27 PM, Mike Spencer wrote:
>>>>>>>>
>>>>>>>>>
>>>>>>>>> I posted a note to uk.rec.sheds (chiefly because someone had used the
>>>>>>>>> word "gubbins" and the Starlite guy recounted calling his product
>>>>>>>>> "gubbins" when first encountered) and had this reply:
>>>>>>>>>
>>>>>>>>>   From: bobharvey <robertharvey at my-deja.com>
>>>>>>>>>   Subject: Re: Sheddi Taxidermy
>>>>>>>>>   Newsgroups: uk.rec.sheds
>>>>>>>>>
>>>>>>>>>   Ah yes.  Starlite.  I recall reading almost exactly that article
>>>>>>>>>   some 20 years ago in some engineering journal.  It included a
>>>>>>>>>   photo sequence of someone stirring molten steel with a stick, then
>>>>>>>>>   putting the stick in a bucket of water without the normal
>>>>>>>>>   dangerous consequences.
>>>>>>>>>
>>>>>>>>>   I always assumed it was all true, unlike the "combustion engine
>>>>>>>>>   that runs on water" man, who used to pop up occasionally.  'cos It
>>>>>>>>>   was clear that that was bollocks.
>>>>>>>>>
>>>>>>>>> If it's bogus, at least it has staying power.  If it's not, why can't
>>>>>>>>> I have some?
>>>>>>>>>
>>>>>>>>> --
>>>>>>>>> Michael Spencer                  Nova Scotia, Canada       .~.
>>>>>>>>>                                                          /V\
>>>>>>>>> mspencer at tallships.ca                                     /( )\
>>>>>>>>> http://home.tallships.ca/mspencer/                        ^^-^^
>>>>>>>>> ______________________________________________________________
>>>>>>>>> TheForge mailing list
>>>>>>>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>>>>>>>> Help: http://mailman.qth.net/mmfaq.htm
>>>>>>>>> Post: mailto:TheForge at mailman.qth.net
>>>>>>>>>
>>>>>>>>> TheForge mail list group photo site is
>>>>>>>>> http://www.photoworks.com
>>>>>>>>> Login: blacksmithblacksmith at hotmail.com
>>>>>>>>> Password: anvil
>>>>>>>>>
>>>>>>>>> This list hosted by: http://www.qsl.net
>>>>>>>>> Please help support this email list: http://www.qsl.net/donate.html
>>>>>>>>
>>>>>>>> ______________________________________________________________
>>>>>>>> TheForge mailing list
>>>>>>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>>>>>>> Help: http://mailman.qth.net/mmfaq.htm
>>>>>>>> Post: mailto:TheForge at mailman.qth.net
>>>>>>>>
>>>>>>>> TheForge mail list group photo site is
>>>>>>>> http://www.photoworks.com
>>>>>>>> Login: blacksmithblacksmith at hotmail.com
>>>>>>>> Password: anvil
>>>>>>>>
>>>>>>>> This list hosted by: http://www.qsl.net
>>>>>>>> Please help support this email list: http://www.qsl.net/donate.html
>>>>>>>>
>>>>>>>
>>>>>>>
>>>>>>>
>>>>>>> --
>>>>>>> Bruce
>>>>>>> NJ
>>>>>>> ______________________________________________________________
>>>>>>> TheForge mailing list
>>>>>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>>>>>> Help: http://mailman.qth.net/mmfaq.htm
>>>>>>> Post: mailto:TheForge at mailman.qth.net
>>>>>>>
>>>>>>> TheForge mail list group photo site is
>>>>>>> http://www.photoworks.com
>>>>>>> Login: blacksmithblacksmith at hotmail.com
>>>>>>> Password: anvil
>>>>>>>
>>>>>>> This list hosted by: http://www.qsl.net
>>>>>>> Please help support this email list: http://www.qsl.net/donate.html
>>>>>>
>>>>>> ______________________________________________________________
>>>>>> TheForge mailing list
>>>>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>>>>> Help: http://mailman.qth.net/mmfaq.htm
>>>>>> Post: mailto:TheForge at mailman.qth.net
>>>>>>
>>>>>> TheForge mail list group photo site is
>>>>>> http://www.photoworks.com
>>>>>> Login: blacksmithblacksmith at hotmail.com
>>>>>> Password: anvil
>>>>>>
>>>>>> This list hosted by: http://www.qsl.net
>>>>>> Please help support this email list: http://www.qsl.net/donate.html
>>>>>>
>>>>>
>>>>>
>>>>>
>>>>> --
>>>>> Bruce
>>>>> NJ
>>>>> ______________________________________________________________
>>>>> TheForge mailing list
>>>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>>>> Help: http://mailman.qth.net/mmfaq.htm
>>>>> Post: mailto:TheForge at mailman.qth.net
>>>>>
>>>>> TheForge mail list group photo site is
>>>>> http://www.photoworks.com
>>>>> Login: blacksmithblacksmith at hotmail.com
>>>>> Password: anvil
>>>>>
>>>>> This list hosted by: http://www.qsl.net
>>>>> Please help support this email list: http://www.qsl.net/donate.html
>>>>
>>>> ______________________________________________________________
>>>> TheForge mailing list
>>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>>> Help: http://mailman.qth.net/mmfaq.htm
>>>> Post: mailto:TheForge at mailman.qth.net
>>>>
>>>> TheForge mail list group photo site is
>>>> http://www.photoworks.com
>>>> Login: blacksmithblacksmith at hotmail.com
>>>> Password: anvil
>>>>
>>>> This list hosted by: http://www.qsl.net
>>>> Please help support this email list: http://www.qsl.net/donate.html
>>>>
>>>>
>>>> -----
>>>> No virus found in this message.
>>>> Checked by AVG - www.avg.com
>>>> Version: 10.0.1382 / Virus Database: 1513/3703 - Release Date: 06/14/11
>>>>
>>>
>>> ______________________________________________________________
>>> TheForge mailing list
>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>> Help: http://mailman.qth.net/mmfaq.htm
>>> Post: mailto:TheForge at mailman.qth.net
>>>
>>> TheForge mail list group photo site is
>>> http://www.photoworks.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> Password: anvil
>>>
>>> This list hosted by: http://www.qsl.net
>>> Please help support this email list: http://www.qsl.net/donate.html
>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoworks.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
>
>
>
> --
> Bruce
> NJ
>



-- 
Bruce
NJ


More information about the TheForge mailing list