Andy,
I don't have the patientce for the small work, plus my eyes aren't so good.
When my son was into making knives and I was going to lots of knife shows.
The makers that did minitures would say that a miniture knife would take as
much work as a full sized knife, but it was hard to get the same price.
Robert Ehrenberger
Shelbyville, Mo.
eforge at centurytel.net
Date: Sun, 04 Dec 2011 08:59:18 -0500
From: Andrew Vida <osan at netlabs.net>
Subject: Re: [TheForge] What are you up to.
To: Bob Ehrenberger <eforge at centurytel.net>, Blacksmithing List
Sounds like a great time. NJBA held and anvil repair event two weeks
ago. I was in NJ but could not get to the event due to transportation
woes. Got there the next day though and it looks like a good time was
had.
Speaking of diagonal pein hammers, I made a wax pattern for one last
night while watching some silly western, "Prairie Fever". It is only
about 3/8" stem to stern and I will eventually cast and helve it along
with the dozen anvils, bottom tools, hammers, and blacksmith's helper I
have sitting around the bedroom.
I have made what I believe to be the world's smallest anatomically
correct London pattern anvil the other day. About 1/4 inch total. I
have one I started just over half that but popped the horn off in a
moment of clumsiness. A little purple wax and all will be good again.
Just not sure if I can manage a hardie hold on that one. Perhaps with
wire EDM after casting... but that is getting a little too psychotic
even for me.
I finished a wrought iron yawara (striking weapon) that has spirally
fluted ends, 1 ball and 1 flame shaped. Light etch to bring out the
grain and soften the edges with a vigorous hand burnishing with a wire
brush.