Jack Brubaker from IN would be the one to contact
Last year he demonstrated scythe blades at the Indiana conference
I did not tape him but possibly IBA did or try contacting Jack direct
I have a couple old scythes and some extra blades. Not very good at it but
it can be fun, and beats the heck out of using a weed whacker.
I've seen ads for the scythe stakes and hammers but never could figure out
the process from the ads. They never had very good pictures. I usually end
up just putting a 600 grit belt on the sander and using that to sharpen my
blades. After hammering the edge was he done, or did he still have to work
it over with a stone?