Mike,
I have a couple old scythes and some extra blades. Not very good at it but
it can be fun, and beats the heck out of using a weed whacker.
I've seen ads for the scythe stakes and hammers but never could figure out
the process from the ads. They never had very good pictures. I usually end
up just putting a 600 grit belt on the sander and using that to sharpen my
blades. After hammering the edge was he done, or did he still have to work
it over with a stone?
Robert Ehrenberger
Shelbyville, Mo.
eforge at centurytel.net
----- Original Message -----
Date: Sat, 27 Aug 2011 18:51:11 -0300
From: mspencer at tallships.ca (Mike Spencer)
Subject: [TheForge] Re:Spring steel (and other) breaking in mild acid
I spent most of today at a hand mowing competition. I wanted to see
if I could pick up some pointers on my style but mainly I wanted to
learn about "peening a scythe blade".