If you use PVC for compressed air it will fail -- the only question is when
and how. Not only is fatigue an issue but oil from the compressor may also
effect the PVC.
There is plastic pipe compounded and design for air system piping -- but you
will need to go to a major plastic pipe supply, or one that sells systems
for shop use to find it -- not your local Big Box store.
Here is one supplier http://www.rapidairproducts.com/ they sell both nylon
tubing and a composite plastic and aluminum pipe and the required fittings.
This is just one source -- other can be found by google on "compressed air
piping"
Dave
--------------------------------------------------
From: "Paul N" <crosspein at sbcglobal.net>
Sent: Tuesday, April 05, 2011 8:33 AM
To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
Subject: Re: [TheForge] PVC for compressed air (A little OT -- a mini-scale
saber saw?)
> I'd be cautious about using PVC for compressed air. For years, there
> have been debates about the danger, and I pretty much disregarded them.
> Then about 10 years ago, I gave in and decided to replace it with type
> "L" copper. Type L is what is recommended for compressed air. Many of
> the big box stores carry it, in addition to the cheaper Type "M", which
> is what is used for the most common plumbing.
>
> The danger of PVC is similar to what is currently in the news for the
> Boeing 737's. The constant flexing from the pressurization and
> depressurization work hardens it over timee and makes it brittle. Then
> it cracks and fails catastrophically, often sending plastic shrapnel in
> all directions.
>
> I became a true believer as I removed the sched. 40 PVC I had previously
> installed. It had been "in service" for about 7 years, and when I pulled
> those pieces down, a number of sections cracked and shattered. They were
> no longer the pliable pipes that they were when I installed them. So,
> unless your plumbing is underground, I'd be very wary of using PVC for
> compressed air.
>
> **paul
>
> On 4/5/11 1:07 AM, peter fels wrote:
>> How much air do you need?
>> More storage means more air for longer.
>> Be very conservative with air pressure tanks!
>> They can go off like a bomb!..Lotta kinetic energy!
>> Putting them somewhere way over there, has a lot of virtue.
>>
>> My first compressor was from an old refrigeration unit,
>> The tubing went to 2, 250 gallon, ( carefully washed out) former propane
>> tanks.
>> I used several hot water heater over- pressure valves in each one and
>> tapped a hole in the bottoms
>> for radiator drain valves .
>> Ordinary sched 40 house plumbing will generally deal with 100 PSI. if you
>> are careful.
>>
>> It was enough air to do a little sandblasting...or run an air tool for a
>> while.
>> Needless to say, that rig took a long time to recover.
>> Safe from air tool boredom.
>> Cost around $5 for fittings i couldn't scrounge.
>>
>> On Apr 4, 2011, at 8:49 PM, Bruce Freeman wrote:
>>
>>> How big a tank do you mean?
>>>
>>> On Mon, Apr 4, 2011 at 6:59 PM, peter fels<artgawk at thegrid.net> wrote:
>>>> An inexpensive little compressor ( even one from a bigger freezer) and
>>>> a big pressure rated storage tank,
>>>> will cover a whole lot of applications.
>>>>
>>>...
> <snip>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge
mailing list