As mentioned before, the amount of loss is dependent on your approach.  I have moved to dry welding in propane fire with multiple re stack.  Lose less than 3% of weight, only re stack once. Please consider some of your options for forge welding.  I am glad to help if you like.  Making pattern welded steel is one of the most exciting and full filling experiences around at least for me.

 

Trusting HIM,
Steve Rollert
keenedgeknives.com
doveknives.com