[TheForge] Forging Tungsten

David E. Smucker davesmucker at hotmail.com
Mon Oct 25 15:39:42 EDT 2010


Are you sure Hofi use Tungsten for tooling?  Or is it that he use a high 
tungsten alloy of steel (steel with high percentage of tungsten) such as T1, 
the original High Speed Tool Steel.  I not sure how to find a higher 
performance material than S7, H11 or H13 for such uses.   T1 is 18 percent 
tungsten, has very heat resistance (as good as H13) good wear resistance 
(better that H13 or S7) but not near the shock resistance of S7.  S7 remains 
my first choice for such tooling,  YMMV.

Dave Smucker
Brasstown, NC

--------------------------------------------------
From: "William Keller" <bkforge at sbcglobal.net>
Sent: Monday, October 25, 2010 10:34 AM
To: <TheForge at mailman.qth.net>
Subject: Re: [TheForge] Forging Tungsten

> Hofi uses it for his hammer punch/slitter and drifts in his press.
>
> Bill
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 


More information about the TheForge mailing list