[TheForge] oil/wax finish, blackened steel

ries ries at riesniemi.com
Sun Oct 24 12:13:53 EDT 2010


yup.

CRS.

ries


On Oct 23, 2010, at 4:59 PM, Andrew Vida wrote:

Did you mean BIRCHWOOD Casey?

ries wrote:
> My buddy James and I did a couple of tables this year that needed blackened- he did the wood, I did the metal- and we found the best way to get consistent results on mixed materials like that was cold, not hot- we sanded all the metal to the same starting point- I used a random orbit sander, with about an 80 grit paper. Then, we used Blackwood Casey cold black, rubbed on with a rag, then rub off the excess. Pretty quickly he clearcoated it, with some fancy imported clearcoat he uses on cabinets. You get a nice consistent finish. 
> I find hot blacking with a torch ok for small stuff, but a big pain for larger items.
> Most all commercial blacking is done in baths, which are hot, but not that hot- 100 degrees or so.
> 
> We have also used commercial gun blueing/blacking liquids from Kesselrings, but they are a lot pricier than buying from Blackwood Casey- a gallon has lasted me about 20 years now of occasional use.
> 
> ries
> 
> 
> 
> On Oct 22, 2010, at 10:53 PM, Robert J Hill wrote:
> 
> Andy,
> Are you using any of the bluing/blackening chemicals first?  The mill  
> scale on the tube can be resistant to the hot wax method.  Maybe a  
> light sanding with 120 grit then scotch brite to take out the sander  
> swirls will help.
> Good luck,
> Rob
> 
> On Oct 22, 2010, at 15:51, Andy Gladish wrote:
> 
> Yikes!
> I'm working on a railing that needs to be finished this weekend, and  
> thought
> I knew how to do a blackened finish...looks fine on the forged stuff,  
> but
> it's a mix of square tube and forged parts and the finish I get from  
> heating
> the steel til the wax mixture smokes when I apply it, is VERY  
> different on
> the tubing than it is on the forged parts...
> Any suggestions, anyone?
> Thanks!
> Andy Gladish
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 
> Ries Niemi
> Industrial Artist
> http://www.riesniemi.com/
> 
> 
> 
> 
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html

Ries Niemi
Industrial Artist
http://www.riesniemi.com/







More information about the TheForge mailing list