I would never try to fix sway unless it was dramatic and accompanied
by numerous other serious defects.  

My PW has just a bit of sway and it helps when straightening.  If I
really need flat to true up some little think, I have a (about)
10"x18" 1-1/4" plate on the bench nearby.

The PW also has no sharp edges.  But I have a piece of (about) 3"x3" maybe
7" long welded to a stake.  It has sharp edges and, put in the hardy
hole crossways, sticks out beyond the edge of the anvil.  It lives
two steps away from the anvil so I can pop it in if I really need a
sharp edge.

FWIW,
- Mike

-- 