[TheForge] Fw: Anvil repair
dan tull
dantull at numail.org
Fri Oct 15 10:44:53 EDT 2010
Exactly what that MG750 rod is.(build up not hard facing)
----- Original Message -----
From: "Jerry Frost" <akfrosty at mtaonline.net>
To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Thursday, October 14, 2010 8:59 PM
Subject: Re: [TheForge] Fw: Anvil repair
> Probably the most common mistake I see is folk using hard facing rod.
>
> If on the other hand you use build up rod like that used in rock crushers
> all you need do is make sure to control the HAZ and heat treat properly
> after it's all over. Build up rod is very much impact resistant but will
> not
> get brittle and sticks to darned near anything. It's intended to build up
> under hardfacing rod, there's a serious limit to how many passes you can
> lay
> with hardfacing rod. One. We used a bunch of both on drill bits, auger and
> such. boy I'm glad I'm not a driller anymore!
>
> Jer
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge