> Probably the most common mistake I see is folk using hard facing rod.
>
> If on the other hand you use build up rod like that used in rock crushers
> all you need do is make sure to control the HAZ and heat treat properly
> after it's all over. Build up rod is very much impact resistant but will not
> get brittle and sticks to darned near anything. It's intended to build up
> under hardfacing rod, there's a serious limit to how many passes you can lay
> with hardfacing rod. One. We used a bunch of both on drill bits, auger and
> such. boy I'm glad I'm not a driller anymore!
>
> Jer
I'm glad you aren't either.
Given a proper heat treat, an arc welded anvil ought to be fine.
Most anvil repairs don't bother.
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>


More information about the TheForge mailing list