[TheForge] spaghetti: blacksmithing content
Bob Smolen
boka at mwt.net
Fri Nov 12 01:18:34 EST 2010
Great looking knocker! I love the wings. How did you make them
Bob
----- Original Message -----
From: "Mike Spencer" <mspencer at tallships.ca>
To: <theforge at mailman.qth.net>
Sent: Thursday, November 11, 2010 12:40 PM
Subject: [TheForge] Re: spaghetti: blacksmithing content
>
>
>> Not long after that a neighbor brought his ram's head poker back to
>> get the point tweaked. Heated the pointy end and laid it on the
>> anvil, and the first time I smacked it the ram's head on the other
>> end popped off and rolled under a table.
>
> I've had some trouble with that, Andy. I've made several door
> knockers like this:
>
> http://home.tallships.ca/mspencer/gallery/img/dragon-knocker.jpg
>
> I'd do the head, then draw out the taper and make the claw. A couple
> of times, as I did the drawing-out, a transverse crack developed near
> the head. The first time it happened, the head fell off, just as
> yours did. [1] The next time, I was able to save the piece by putting
> a deep arc weld into the crack and peening it down but it didn't make
> me happy.
>
> I attributed the failure to (first) multiple reheating of the neck to
> too low a heat, trying to avoid burning the finished head detail and
> (then) continued vibration of the cold part from pounding on the other
> end. And I didn't have to use tensor analysis to imagine that. :-)
>
> Of course, I have -- or had -- an excessively high opinion of my own
> ability to imagine how/why things happen. I had a carefully
> constructed mental image of just how my hammer traveled when I was
> forging. Even wrote up a description once. Then I got a chance to do
> high-speed photography of myself hammering. [2] The hammer flight path
> was nothing at all like the mental construction I had formed. A
> little mortification now and then, they say, is good for us. ;-)
>
>
> Ho hum,
> - Mike
>
>
> [1] Um, your poker ram's head, that is.
>
> [2] http://home.tallships.ca/mspencer/hammer.html
>
> --
> Michael Spencer Nova Scotia, Canada .~.
> /V\
> mspencer at tallships.ca /( )\
> http://home.tallships.ca/mspencer/ ^^-^^
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
--------------------------------------------------------------------------------
No virus found in this incoming message.
Checked by AVG - www.avg.com
Version: 8.5.449 / Virus Database: 271.1.1/3250 - Release Date: 11/11/10
07:34:00
More information about the TheForge
mailing list