If it is small enough, use a wire wheel, but sandblasting is the best
way to remove scale. Also use a heavier acid like muradic also named
hydrochloric. It has a horrible smell, will burn an open wound, but I
use it when I solder galvanized and it burns ygr galvanize off almost
instantly and leaves a clean scale free steel finish. It dilutes in
water and use baking soda for clean up.
On 3/30/10, ries <ries at riesniemi.com> wrote:
> Most likely the problem is that you still have mill scale on the
> material.
> For a good rust finish, you need to sandblast first- its the perfect
> mix of a slightly toothy finish, clean, with no mill scale.
> I find that if you sandblast, it will rust with just a bit of salt
> water- rock salt dissolved 10 to 1 or 20 to 1 in a windex bottle.
> The problem with bleach or peroxide is once it starts, it doesnt stop,
> it just keeps rusting under whatever you put on top.
> Salt water is easier to stop, I find.
> Neutralize any of em with a baking soda/ water mix.
>
> wire brushing or sanding will help, not as good as sandblasting, but
> workable.
> Or a tumbler.
>
> ries
>
>
> On Mar 30, 2010, at 3:21 PM, Mark A. Pesetsky wrote:
>
> What about bleach?
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Allen Ortery
> Sent: Tuesday, March 30, 2010 6:14 PM
> To: theforge at mailman.qth.net
> Subject: [TheForge] finish problem
>
> I was trying to use peroxide to put a rust finish on some iron but it
> did not work, what did I do wrong? First cleaned in PH minus then
> scrubbed with scotch brite pad under clean water got rid of excess water
> and spray with peroxide. Nothing happened, peroxide to week?
> Allen
>
>
> --
> Allen Ortery
> bluestoneforge at gmail.com
> 309-368-7967
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
> Ries Niemi
> Industrial Artist
> http://www.riesniemi.com/
>
>
>
>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
--
Sent from my mobile device
John Allen
Country Metals, LLC
(856) 542-4316 (cell)
(856) 504-0087 (fax)
More information about the TheForge
mailing list