[TheForge] Fume and chemical esposures

David E. Smucker davesmucker at hotmail.com
Mon Mar 22 15:05:31 EDT 2010


There has been some on going work in this area -- could be better.

There has been a link shown between "welders" and an increase risk of 
Parkinson's.  How strong the link is I don't know.
Keep out of the fumes.

Dave

--------------------------------------------------
From: "Peter Fels & Phoebe Palmer" <artgawk at thegrid.net>
Sent: Monday, March 22, 2010 1:14 PM
To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
Subject: Re: [TheForge] TheForge Digest, Vol 74, Issue 17

> Given so many of us have extensive exposures, someone ought to be making
> up a data base and tracking our health. It'd be real useful.
> For example, I've 3 ex welder friends with Parkinson's just now.
> My own exposures and medical history cover pages.
>
> John Husvar wrote:
>>
>>
>> On 3/21/10 8:33 PM, "Jerry Frost" <akfrosty at mtaonline.net> wrote:
>>
>>
>>> extravagant sounding precautions. Xylene is BAD for you, really BAD.
>>>
>>
>> So _that's_ what happened to me! Now I know why I'm so craaaaazy, crazy
>> enough to be a smith anyway! :)
>>
>> When I worked in the overhead crane factory and for a crane service 
>> company
>> we used Xylol (trade name for xylene) for parts cleaning and darn near
>> everything else as a solvent, thinner and so on; no wimpy gloves, suits,
>> respirators, etc.:)
>>
>> Hell, it was also a factory joke to tell a guy to be careful using MEK to
>> degrease gearboxes etc. and laugh at him when he passed out if he didn't 
>> pay
>> attention. (Losing consciousness without warning is a known hazard of 
>> MEK.)
>>
>> It's a wonder I've lived _this_ long. I've provably (not probably) been
>> exposed to nearly every industrial chemical and hazardous material there 
>> is
>> and with little or no protective gear. I'd bet there isn't one plant I 
>> did
>> repairs in that wasn't loaded with asbestos. It was the industry standard
>> insulation back in the day.
>>
>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 


More information about the TheForge mailing list