[TheForge] blackened steel finish

Jerry Frost akfrosty at mtaonline.net
Fri Jun 25 18:42:33 EDT 2010


Phosphoric acid will produce a durable flat black finish but it can turn 
white in spots depending on humidity and such. Ospho is a commercial 
phosphoric acid etch rust converting primer that works well.

frosty
-------------------------
If it ain't forged
It ain't real
wrought iron is
The Frostworks



----- Original Message ----- 
From: "Lucky7Steel" <lucky7steel at gmail.com>
To: <theforge at mailman.qth.net>
Sent: Friday, June 25, 2010 6:16 AM
Subject: [TheForge] blackened steel finish


> Anyone have any suggestions for getting basically the mat finish of
> hot rolled on cold rolled steel?
> I have trouble finding Patina's in Toronto.
> suggest?
>
>
> ~Karen~
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html 



More information about the TheForge mailing list