It depends on what drill style you have and angles but I cut the bits
down to 3 inches long or enough so they can't wable. You lose the bit
but gain a lot of time.
On 1/28/10, Peter Fels & Phoebe Palmer <artgawk at thegrid.net> wrote:
> Andy...i grind a spot that's perpendicular to the hole to be drilled,
> then centerpunch and drill pilot hole
>
> Andy Gladish wrote:
>> Slap me if I've asked this already, but this forum seems to be the best
>> bet for getting feedback of any I've found out there...
>> Anyone care to walk me through drilling angled holes? I've tried pilot
>> holes of various kinds, but I set up the drill press at 34 deg, and can't
>>
>> figure out how to get the 1/2" bit started so it digs in in exactly the
>> right place- drilling an approximate hole isn't that hard, drilling an
>> accurate one is so far impossible. The bit wants to wander off down hill
>> no matter what I"ve done.
>> Signed,
>> Stumped in Seattle
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
--
Sent from my mobile device
John Allen
Country Metals, LLC
(856) 542-4316 (cell)
(856) 504-0087 (fax)
More information about the TheForge
mailing list