Once there's live rust under a finish in a damp 
place..that's usually that, and it'll lift the finish in 
time...Unless you chemically convert the rust to a more 
stable form...and functionally, that's iffy.
Iron expands a whole lot as it rusts.
Think it was designed mostly for Cu alloys.

Andy Gladish wrote:
> In my case it proceeded to rust badly, within a couple months, through two 
> brushed coats. I don't have spray equipment and I like hand brushing, spent 
> some years painting wealthy peoples' homes. I thought I did a good job 
> degreasing with acetone....
> Used it over light rust on a gate and it seems to be alright, mostly- but it 
> sure hasn't lived up to what I was told about it...will have to take it up 
> with the maker, perhaps I missed something crucial.
> 
> --------------------------------------------------
> From: "Cindy and James" <jallcorn at suddenlink.net>
> Sent: Friday, August 13, 2010 5:41 AM
> To: <theforge at mailman.qth.net>
> Subject: [TheForge] Permalac
> 
>> Re the comments on Permalac .  If the patina/finish is thick, as in
>> crusty, etc. for lack of better term, SPRAY the permalac using multiple
>> coats to penetrate and seal the patina.
>>
>> Many patinas are extremely fragile and must be treated with much care in
>> the sealing/lacquering process.  I have found this out via experience.
>>
>> James
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html 
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 


More information about the TheForge mailing list