[TheForge] Chemicals- trials and tribulations
Peter Fels & Phoebe Palmer
artgawk at thegrid.net
Thu Aug 12 23:15:22 EDT 2010
I did brush it Andy, but mine failed cause the patina
underneath lifted off.
I'd foolishly hoped that the permalac would sorta stick
it down or hold it in place by the film strength....WRONG!
Whenever i had a dry, solid substrate, it did just fine.
On the bottle openers, corkscrews and belt buckles it
held up well...a good test.
Andy Gladish wrote:
> Very interesting thread- I was really excited about P-lac but it failed
> badly when I used it on a couple of bright new expanded metal tabletops
> (patio furniture).
> Pete, more about why yours failed- was it the brushing, cuz I brushed mine.
> Andy
>
> --------------------------------------------------
> From: "Lucky7Steel" <lucky7steel at gmail.com>
> Sent: Sunday, August 08, 2010 8:15 PM
> To: <theforge at mailman.qth.net>
> Subject: Re: [TheForge] Chemicals- trials and tribulations
>
>> Very interesting. thanks for all the info.
>> Confusing though because isn't it an acid? If i don't rinse it off doesn't
>> it just keep on ....blackening?
>> I'll give a try just wiping then waxing though. I dont always have access
>> to
>> all the chemicals mentioned here because i live in Canada and i'm lucky to
>> have figured out where to get the JAX i think! Can't get most things
>> shipped
>> dues to the Haz Mat status of a lot of these chemicals.
>> On the chemicals side, has anyone tried Permalac spray laquer? I use
>> Tremclad but i find it to suck mostly.
>>
>> ~Karen~
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge
mailing list