[TheForge] Bronze

Peter Fels & Phoebe Palmer artgawk at thegrid.net
Thu Aug 5 15:07:51 EDT 2010


Kim;
I have a vague recollection that certain bronzes actually 
harden on quenching..not sure which ones though.

Kim George wrote:
> I find that I have the tendency to hit that piece one time too many.
> So by quenching I'm covering my bases. most of the bronzes are not
> hurt by this and at the right temp it moves so much I figure some
> stress  is inherent.
> 
> On 8/5/10, Peter Fels & Phoebe Palmer <artgawk at thegrid.net> wrote:
>> Jim;
>> When you say you can't anneal Cu alloys without having
>> cold worked it...
>> Is that because it's already annealed from the hot
>> working temperature?
>> That's what i'd been assuming.
>>
>> James Binnion wrote:
>>> On Aug 4, 2010, at 7:52 PM, Kim George wrote:
>>>
>>>>  You should also quench it
>>>> about every third time. Re member when you do that you are annealing
>>>> the piece.All nonferrous metals are like that.
>>> This is not right. Annealing of any metal or alloy comes from heating
>>> it past the point of stress relief and into the recrystallization
>>> temperature range. Where that temperature range is depends on the
>>> physical properties of the alloy or metal and how much cold work you
>>> have put into it, the more cold work the lower the temperature. Not
>>> enough cold work and you will not be able to anneal it. If you are hot
>>> forging the work and do not put any cold work into it you cannot
>>> anneal it, you can heat it to the point of crystal growth (which is
>>> generally a bad thing) but you will not get recrystallization.
>>>
>>> Some alloys care about how you cool them after annealing and some
>>> don't. Some need a rapid quench some need a slow cooling and with some
>>> it just don't matter. Non ferrous metals vary in what is needed just
>>> as ferrous ones do. If in doubt look it up, the internet is full of
>>> alloy data sheets that have hot work temperatures, annealing
>>> temperatures and other useful info.
>>>
>>>
>>>
>>> James Binnion
>>> jbin at well.com
>>>
>>>
>>>
>>> ______________________________________________________________
>>> TheForge mailing list
>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>> Help: http://mailman.qth.net/mmfaq.htm
>>> Post: mailto:TheForge at mailman.qth.net
>>>
>>> TheForge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> Password: anvil
>>>
>>> This list hosted by: http://www.qsl.net
>>> Please help support this email list: http://www.qsl.net/donate.html
>>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
> 
> 


More information about the TheForge mailing list