bright is the wrong look. it could be stainless which is almost
impossable to forge weld. does a magnet stick to it? also do you twist
it tight while it is in the cherry range. first this I do is heat flux
twist. then bring up to wielding heat. if you have a v block it makes it
much easier to not blow it apart .
On 8/3/2010 11:20 PM, FireWorks PDX wrote:
> I have a length of bright steel cable (1-1/2" diameter) that I want to forge weld into a solid base for a sculpture. I'm using Z-weld flux. My first attempt failed, I think due to a lack of heat, but I dunno. Maybe I'm not getting flux in between the threads? Any advice? I'm going to check through Zoeller's site, too, but I figured sending it out to y'all might help.
>
> Thanks,
> Mark
> Fireworkspdx.com
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge
mailing list