> Mike Spencer wrote:
>> C
>>
>> One guy here ran out of coal. For a stop-gap, he's been starting a
>> good fire in his barrel stove, then stuffing if full of wood and
>> bunging it up tight for the night. The next day he has some half-fast
>> (sp? Or is that half-baked? :-) charcoal. Says it works pretty good
>> in the forge.
>>
>>
>>
>>