[TheForge] making shovels ... me too?
Paul N
crosspein at sbcglobal.net
Wed Mar 4 16:24:45 EST 2009
Please post response here. I'd like one too.
I recently hammered one out of a piece of 1/2" x 1 1/2" x 4"
(free-hand). It came out pretty nice, despite the wear on my arm. (Talk
about your forging contest). It looks quite rustic, but I'd like to try
and make a more consistent shovel
Allen Ortery wrote:
> I am mad at myself for being stupid and not making a copy of the form
> and the shovel blank that we used at the John c. campbell Folk school
> when I was there. Does anyone have the plans for the one that francis
> Whitaker used? It hangs on the back wall in the shop there. I really
> like that one and the way it looks.
> Any help would be great.
> Thanks Allen Ortery
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
>
More information about the TheForge
mailing list