I primarily spray everything since there is very minimal spatter. I
use a 92 argon 8 CO2 mixture. Electrode positive for mig welding and
negative for flux core. 75 25 is ok for spray, its best advantage is
lower spatter in short circuit.
On 3/2/09, Woolley <wjec1 at verizon.net> wrote:
> Peter,
>
> Bare wire Mig is DC reverse polarity (positive electrode), flux core is
> strait polarity. 75/25 mix is ideal, all positions. Some good info here:
>
> http://www.welding-advisers.com/Mig-welding-tips.html
>
> Good luck
>
>
>
>
>
>
> Peter Fels & Phoebe Palmer wrote:
>> Been trying to figure out MIG spray deposition now that i have the power
>> to do it.
>> Using .035 wire and argon75% CO2 25% mix gas. Electrode negative.
>> If i crank it up to about 400 ipm and about 25 volts i get spray
>> deposition as i imagine it to be, but the nozzle and contact tip seem to
>> foul pretty quickly.
>> Part of the problem was the awkward position of the welds and a sore
>> back...which contributed to the fouling i'm sure.
>> Looking on the web, they were talking about a different gas mix ( i was
>> using what i have and can easily get) and electrode positive setting.
>> Is that right? I keep imagining the wire fusing to the contact tip as
>> soon as the trigger is pulled with electrode pos.
>> Can the gas i have be made to do spray deposition decently?
>> Sure appreciate having you folks around to straighten my path every now
>> and then...pete f
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
>>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
--
Sent from my mobile device
More information about the TheForge
mailing list