[TheForge] fire clay

Allen Ortery bluestoneforge at gmail.com
Sun Jun 7 11:06:12 EDT 2009


try packable refractory, they use it to repair boilers. holds up very
well. should be able to get it at plumbing and heating supply.

-- 
Allen Ortery
bluestoneforge at gmail.com
309-368-7967