My guess would be that the titanium is just a coating.

I like the Duluth Trading catalog.

Bob
____



On Jul 31, 2009, at 7:34 AM, Jeff & Leslie wrote:

> Morning,
>
> I bought a couple of shirts from the Duluth catalog and was  
> convinced to buy
> em by the promise of a titanium blade knife for FREE.  The knife  
> really
> ain't bad for a freebie chineese knife.  Blade is a hokey rainbow  
> color.
> has the tiny ball bearing that helps it open.  I was surprised that  
> the
> blade is magnetic.  Must be mostly steel.  So my question is how much
> titanium is there in a titanium blade?   Did the chineese just wave  
> this one
> over the pot of titanium?  Is there an optimum percentage?
>
> Inquiring minds are wondering.
>
> Thanks,  Jeff Valentine