[TheForge] cutting off copper ferrules?
Bruce Freeman
freemab222 at gmail.com
Tue Jul 28 17:02:44 EDT 2009
I thought this was going to be a simple task, but maybe I didn't
reckon with copper.
I need to use 1/2" (nominal, actually about 5/8" OD) copper water
tubing to make a bunch of ferrules. For reasons I won't go into, no
other material will do, I'm stuck with copper tubing. I tried
chucking a piece in the lathe and parting it off, but no go. I'm not
sure what was wrong, but I could not get any sort of clean cut.
Since then I've been using a power hacksaw and LOTS of clean-up work
with files. I'd like to find something better.
I'd love to use a roller cutter, but I can't tolerate the ID reduction
those things give. Otherwise, this is not precision work. All I'm
doing is making some ferrules.
Any idea? (A solution involving the lathe is not essential.)
--
Bruce
NJ
The total lack of evidence is the surest sign that the conspiracy is working.