[TheForge] welding red brass, slightly OT
ries
ries at riesniemi.com
Wed Jul 1 12:20:01 EDT 2009
Jim is right- C230- I got my two's and three's mixed up.
sorry.
ries
On Jul 1, 2009, at 9:17 AM, James Binnion wrote:
If it truly is red brass which is the old trade name for C2300 which
is 85% copper 15% zinc you can oxyacetylene or TIG it but it has a
tendency to fume. It is rated as only "Good" for those two welding
processes and not recommended for stick you could probably MIG it
with argon shield gas but I don't know where you would get the wire.
Brazing is better but then there is the color mismatch issue with the
filler material.
FWIW
James Binnion
jbin at well.com
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
Ries Niemi
Industrial Artist
http://www.riesniemi.com/
More information about the TheForge
mailing list