Seems to me that large construction failures .. like occurred in the
Boston Tunnel are often to do coruptions, where substandered matterials
like poor quality concrete are fraudulently substituted for the quality
matterials intended and paid for.
In the rural areas, reputation is so important: the word of mouth is
such that a company doing shoddy work, or using substandered materials
won't be in business very long.
Had a friend from Denver, Colorado tell me that when he had his home
re-shingled. They stripped everything down to the plywood sheeting. Most
of the 4 by 8 sheets of plywood were originally only nailed with one nail
in each corner.. just 4 nails to a sheet of plywood. The contractor
doing the reshingling found some other "short cuts" that needed rework,
turned into a lot of additional cost for the homeowner.
The original carpenters and forman that over saw work were likely 15 or
more years beyond prosecution. I think those of us that build for
ourselves tend to "over build", but if it looks like a Do it yourself
construction, the inspectors look much closer at us, than the
"professionals" that know how to cover their shoddy work.
Dann
> Your right Jerry. In Ohio, Ag buildings are not considered commercial or
> residential so they are not covered. I too am on a farm ... my shop is
> non commercial and supports my farm use so it is an ag building.
>
> I just wanted others to be aware that in Ohio, even rural areas are
> covered under the commercial code. A few years ago, I worked hard to keep
> a guy from going to jail in Loudonville. He had been told by the local
> residential building department that there was no commercial building
> department so he didn't need a building permit. The judge said it didn't
> matter what the inspector told him and that it was still his
> responsibility.
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list