[TheForge] rust finish
Peter Fels & Phoebe Palmer
artgawk at thegrid.net
Thu Jan 8 22:36:08 EST 2009
I am Wayne;
At my last place, 20 ga would perforate in a year..but that severity
drops off pretty quickly as you get back from the surf.
Except for road salt exposure, i wouldn't even consider paint there
myself. Cold shuts and overlaps may be one exception, thin intricate
work is another...fusst clients yet another.
Where it's warm and wet and salty is where the corrosion is max.
Unless you have delusions of immortality; stout, unpainted steel does
reasonably well.
Steel is transient and so are we...pf
Wayne Ackman wrote:
> Really, and you are out by the coast, IIRC, I'm at the Four Corners,
> which most years thinks its a desert, except for the last couple with
> snow up to our eyeballs.
>
> Wayne Ackman
>
>
>
>
>
> On Jan 8, 2009, at 1:34 PM, Peter Fels & Phoebe Palmer wrote:
>
>> I will note that i've long advocated a natural rust finish and
>> unprotected exterior pieces i put in 30 years ago are still intact..pf
>>
>> Wayne Ackman wrote:
>>> Yeah, and I can promise him to hold the line at just double the price
>>> for the replacement.
>>>
>>> Wayne Ackman
>>>
>>>
>>>
>>>
>>>
>>> On Jan 8, 2009, at 1:26 AM, Peter Fels & Phoebe Palmer wrote:
>>>
>>>> Wayne;
>>>> Why finish it at all if he wants a natural look? Unless you used
>>>> very
>>>> light material or it's right by the ocean, brush it and rust it and
>>>> shake his hand. Then sell him a replacement in 20 years.
>>>>
>>> _______________________________________________
>>> Manage membership or unsubscribe at:
>>> http://mailman.qth.net/mailman/listinfo/theforge
>>> theforge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> password: anvil
>>> ___________
>>>
>>>
>>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list