Ruuf, 

 

Try a circular saw with the cutting depth set just a couple of mm deeper
than the material you are cutting. I think you will find even the cheaper
blades will last longer, cut faster and there is less wear on the tool.

 

Ron C

 

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Ruuf
Sent: Friday, January 30, 2009 4:52 PM
To: Blacksmithing List Sponsored by ABANA
Subject: [TheForge] Cutting Technique

 

Been cutting some 6mm plate with my angle grinder. I notice sometimes I wear
the cutting disc out rather rapidly. Is there a best industry practice /
technique?





****************************************************************************
********
This footnote confirms that this email message has been scanned by
PineApp Mail-SeCure for the presence of malicious code, vandals & computer
viruses.
****************************************************************************
********







 
 
************************************************************************************
This footnote confirms that this email message has been scanned by
PineApp Mail-SeCure for the presence of malicious code, vandals & computer viruses.
************************************************************************************


-------------- next part --------------
An HTML attachment was scrubbed...
URL: http://mailman.qth.net/pipermail/theforge/attachments/20090202/07cfef34/attachment.html 


More information about the TheForge mailing list