I'm not a weldor, so I can't make a recommendation, but Lincoln
Electric's "The Procedure Handbook of Arc Welding" devotes about a
chapter and a half to the problem of distortion and its control.
On Mon, Apr 20, 2009 at 11:30 AM, Andy Gladish <gladish at cablerocket.com> wrote:
> Would anyone like to suggest a good metal fab book that discusses
> controlling distortion due to cooling welds?
> I've been doing it on the fly for some years now, I bet there's a world of
> better techniques than what I use.
> Thanks for any ideas!
> Andy G.
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
--
Bruce
NJ
The total lack of evidence is the surest sign that the conspiracy is working.
More information about the TheForge
mailing list