[TheForge] low carbon sheet

Peter Fels & Phoebe Palmer artgawk at thegrid.net
Mon Sep 15 05:04:31 EDT 2008


An additional note here..that old fired enamel is often leaded.  pf

Andrew Vida wrote:
> Deep draw sheet should be called AXDQ, IIRC.  There are also newer, 
> supposedly superior steels as well.
> 
> A good place to find deep draw sheet is the scrap yard or the curb. 
> Washers, dryers, refrigerators, freezers, and stoves (non-stainless) are 
> all made from it.  That is, their outer structures.  the one problem may 
> be getting the enamel off.
> 
> Peter Fels & Phoebe Palmer wrote:
>> Jim;
>> Look for deep draw sheet if you can find it. Otherwise, i read that 
>> the sheet they used to enamel for stove sides is pretty close.
>> The sheet they use to make laminated motor cores, transformers and 
>> electromagnets ought to be good, but i don't know where to get smaller 
>> amounts...pf
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 


More information about the TheForge mailing list