[TheForge] Top of a broken anvil
A Vida
osan at netlabs.net
Wed Sep 10 20:32:18 EDT 2008
Tai's hammer control is absolutely phenomenal. Rival's that of guys
like Peter Ross - no joke.
Jonathan Barnhart wrote:
> I've seen what Tim and Marian can do. I've also seen the whole Neo-Primitive process for blade making as done By Tai Goo, Tim, Marian, and others. I like the sentiment. I use anything that I can recycle(especially if I can get it for free or already have it on hand). However, I'm leary of using concrete in this capacity. The Anvils that Tim and Marion use look like shrinks and spalls could be quickly repaired. It would be as simple as mixing more concrete and filling the holes as they came up. In their case the anvil is a long rectangular block which would help hold it. In my case it would probably be smaller and would probably loosen and be hard to fix without starting over.
>