Sorta off topic but I can attest to the exploding butane lighter in the 
pocket story.  I know a guy whose wife won a pretty hefty lawsuit from 
Bic or one the companies that make the lighters after one of them 
exploded in her pocket and took a pound of flesh or so with it. This was 
18-20 years ago. No joke.








Ron Childers wrote:
> Didn't need to anneal as I left it as-is and didn't try to forge a flare,
> but that would work harden it. I drilled the primer pocket and tapped for
> the forged handle/scrolled hook then welded a chain onto a ball bearing for
> the clapper. I did anneal the bearing several times but does anyone actually
> KNOW of a bearing exploding because of welding? Maybe it's like the machine
> gun barrel cut in two with a sword or the plastic lighter exploding in a
> weldor's pocket- we have heard of it but not actually seen it.
>
> Ron C
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Andrew Vida
> Sent: Thursday, October 02, 2008 9:22 PM
> To: Blacksmithing List Sponsored by ABANA
> Subject: Re: [TheForge] RE: Tarnished brass
>
> I could be wrong, but I don't think that you want to anneal the metal in 
> a bell.  It will certainly alter the tonal characteristic, and I am 
> fairly sure that it will dull it.
>
> Peter Hirst wrote:
>   
>> Annealing brass:  dull red & water
>> quench.
>>
>>
>> ----- Original Message ----- From: "Franklin Police" <780 at mchsi.com>
>> To: <munlaw2 at hcsmail.com>; "'Blacksmithing List Sponsored by ABANA'" 
>> <theforge at mailman.qth.net>
>> Sent: Thursday, October 02, 2008 5:48 PM
>> Subject: RE: [TheForge] RE: Tarnished brass
>>
>>
>> Not sure about brass but to clean copper we use HTH brand PH minus from
>> Walmart.
>> Mix the powder with hot water and let soak in plastic bucket.
>>
>> Did you anneal while making the bell
>> I bought a few shells and was thinking about doing some trench art with 
>> them
>> like I do copper pipe.  Anyone have suggestions on annealing?
>>
>> Roger R Degner
>>
>>
>>
>>
>> What is the quickest way to clean tarnish off a brass 90mm cannon shell? I
>> made a bell out of it and would like to shine it up, but Brasso hardly
>> touched it.
>>
>> Ron C
>>
>>
>>
>>
>>
>>
>>
>>
>>
>>
>>     
> ****************************************************************************
>
>   
>> ********
>> This footnote confirms that this email message has been scanned by PineApp
>> Mail-SeCure for the presence of malicious code, vandals & computer
>>     
> viruses.
>   
> ****************************************************************************
>
>   
>> ********
>>
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>>     
>
>   



More information about the TheForge mailing list