[TheForge] Safety -- Turning Things Off topic
Andrew Vida
osan at netlabs.net
Tue May 27 19:52:33 EDT 2008
Peter Fels & Phoebe Palmer wrote:
> Good sirs;
> I like machinery too,and the first few exchanges were interesting...but.
>
> BS then.
> I've been forging 304(?) scrap stainless recently and the cold shuts and
> their propagating cracks are getting frustrating. Same with some bronzes
> and tool steels.
> Especially true when extensive upsetting is called for.
> I end up spending time grinding out the surface flaws, flaps, nicks and
> so on, isn't all that much fun.
> Help, hints or expositions please......pete f
One thing to be aware of is that stainless needs a greater soak time
than mild steel. It absorbs heat comparatively slowly.
--
-Andy V.
no .sig
go .fig