Wow.  So many replies, so many useful suggestions.  Thanks to all.  As 
usual, as many solutions as smiths.  One of the things I love about this 
craft!!!

 By way of explanation/clarification.  The lead around the nubs is in leaf 
form, not melted and poured, so I am assuming there is at least a little 
potential play in it somewhere.  The hole saw is actually an intriguing 
idea:  this is literally a square peg in a round hole,and the hole saw might 
just get the lead out.  Nubs are about 5/8 - 3/4 square.

Heat:  yes, I was thinking a torch, a small heating tip concentrated on the 
center of the exposed nub of iron.  Problem is yes the stone is a heat sink 
and since this is lead, not solder, I am assuming a melting point of 620 F 
and change, not the 400 range. Anyone know what temperature short of melting 
lead would soften  significantly to allow a little wiggle in the iron nub? I 
really dont want to mess with rock and heat, and I think I would rather 
destroy and replace the nubs than risk the stone.  But if it could be done 
at a low temp, it might be an ok last resort.

Slide hammer:  to pull only, straight up,  never to strike.  To pull either 
on vise-grips clamped on the nub (they are about 1/4 above flush cut)  or on 
a stud remover or bolt tapped and sunk in the nub.

Brazing vs welding:  Since the joint is about 1/4 above flush it will be 
exposed, and I would like to keep it as original as possible.  I would also 
like the owner to be able to say that the  boot scrapers are all as original 
as possible, even if the part below grade is a bit of an abstraction.  I 
will be giving them a provenance with the repair, and they will be giving 
the contractor the bill.

Keziah



----- Original Message ----- 
From: "Ron Childers" <munlaw2 at hcsmail.com>
To: "'Blacksmithing List Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Wednesday, May 07, 2008 4:01 PM
Subject: RE: [TheForge] Repair job


Wasn't the Stone Mountain sculpture done by controlled application of heat?
Made a hellova racket when the rock exploded. I could hear it from quite a
distance.

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Andrew Vida
Sent: Wednesday, May 07, 2008 3:54 PM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] Repair job



Peter Hirst wrote:
> I have been asked to repair a pair of antique boot scrapers that an idiot
contractor
damaged in a sill replacement job.  1719 house with the matched pair
nicely leaded
into the granite front step.  In replacing the sill, idiot (or worse)
contractor
cut the boot scrapers off (not quite flush) rather than move the step.

    !!!  Holy crap.  My skin crawls as I type.

 > I have thought of three ways to do the extraction of the remaining
nubs:

(1) vise grips and slide hammer (preferred),

    Hmmm... not sure what you mean here exactly, but if it is what I
think
it is I would be careful.  What kind of stone is it in?  If you try to
brute-force it out you may cause the stone to fail in some measure
around the hole, which is probably not acceptable.  Don't make worse the
idiot's blunder.


(2) stud extractor and slide hammer ( would rather avoid drilling out
the original nubs);

(3) heat (prefer not to destroy the original lead or risk cracking the
stone: they are 3 inches from the edge.

    I may be wrong, but I would think that forcing it out with a slide
hammer is more likely to break the stone than heat, if done very
carefully.  If the stone is granite, I would not worry that much about
spalling.  Porous stone like limestone will spall terribly if there is
any moisture in it.  The problem with a well installed piece of iron is
that it is a bitch to remove.

    Could you drill them out with a diamond core drill?  Sink the hole
and
then wedge it loose from one side and dress the bottom.  Break the stone
away from the lead in the core, melt  off the lead, and there is your stub.
>
> Also, the weld itself seems tricky.   I am inclined to use gas to reattach


the nubs:  They must be butt welded and SOLID to retain shape and
structural

integrity.

    How about forging a socket that accepts the severed ends of the
scraper?  You can make it from wrought iron and either solder it onto
the scraper or forge weld it.  Like so:

         _        _
                 / |      | \
                /  |      |  \
                |  |      |  |
                |  |      |  |
                |  |      |  |
                |  |______|  |
                |            |
                |            |
                |            |
                |            |
                |__        __|
                   |      |
                   |      |
                   |      |
                   |      |
                   |______|


    If you do the weld correctly, you will have a meaty extension that
can
be forged to shape as needed.  I would think this to be the safest and
most structurally effective means of affecting the repair.  You don't
even have to make a socket, just a yoke (socket minus two sides).  It
would weld more easily and be plenty strong enough.

    If you end up with something slightly different below the lead line,

who cares... as long as it is strong and secure.

  Forge weld seems dicey considering the weld is at the point that

    See above. :)

> Any advice  welcomed.  I can post pics if there is interest in this
project.
-- 

    -Andy V.

no .sig
go .fig
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________



_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________




More information about the TheForge mailing list