[TheForge] Repair job

Ron Childers munlaw2 at hcsmail.com
Wed May 7 10:35:27 EDT 2008


At what temperature does granite spall or discolor? Is there room to drill
out the lead, repair the scrapers and re-pour the lead? Without looking at
it, that seems the safest way to accomplish the job. 
Ron C

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of dan tull
Sent: Wednesday, May 07, 2008 10:09 AM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] Repair job

Torch?
----- Original Message ----- 
From: "Peter Hirst" <saltydog335 at aol.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Wednesday, May 07, 2008 8:08 AM
Subject: [TheForge] Repair job


I have been asked to repair a pair of antique boot scrapers that an idiot 
contractor damaged in a sill replacement job.  1719 house with the matched 
pair nicely leaded into the granite front step.  In replacing the sill, 
idiot (or worse) contractor cut the boot scrapers off (not quite flush) 
rather than move the step.  I need to remove the nubs, reweld them to the 
scrapers and reinstall.  Anyone have any experience with R&R of lead-mounted

iron in stone?  I have thought of three ways to do the extraction of the 
remaining nubs:  (1) vise grips and slide hammer (preferred), (2) stud 
extractor and slide hammer ( would rather avoid drilling out the original 
nubs); (3) heat (prefer not to destroy the original lead or risk cracking 
the stone: they are 3 inches from the edge.

Also, the weld itself seems tricky.   I am inclined to use gas to reattach 
the nubs:  They must be butt welded and SOLID to retain shape and structural

integrity.  Forge weld seems dicey considering the weld is at the point that

gets nearly all the stress in use.  Is pure iron filler rod avaialble, or am

I ok with ordinary mild steel rod?  One of the scrolls needs to be replaced,

but I am ok with a forge weld for that, since its a faggot weld along about 
a 3" surface.

Any advice  welcomed.  I can post pics if there is interest in this project.

Keziah
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________


_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________





More information about the TheForge mailing list