What is the vise made of?  Given the location of the breaks, it sounds 
like it must be cast iron.  I cannot imagine a wrought vise breaking 
like this without being horribly mangled in the process... unless it was 
poorly manufactured, that is.

The scissor mechanism indicates a parallel jaw arrangement.  Could be 
very nice.

Ben Barrett wrote:
> Howdy, I've got a question about an unfamiliar post vise which I just
> picked up today at an estate sale.
> It is medium-sized, prolly 80 or 90 pounds originally (what I have is
> 75#), with 5 1/2 inch jaws, but the post was broken more than once I'm
> guessing.  The main body, the upper 2 feet, is what I have, although
> the outer upright has also been broken a few inches from the bottom.
> The design variation that is unfamiliar is a hinged cross-member ("X")
> where the usual spring is, and it looks like the bottom end had a
> spring holding it together.  The X fit into a slotted piece on the
> main post and the front [partial] post.  The threading appears to be
> in great shape and the jaws line up real nice aside from normal wear,
> so I am hopeful about mounting this on a stump or even restoring the
> post.  I'll go look for a name on it and could get some pictures
> posted, but I could not find a similar design very easily via google.
> So one break was on the main post, 2' from the top of the jaws, and
> the other is in the front upright member, which is a sort of channel
> on this vise.
> Woohoo, I got the vise, some good old USA-made tools (pipe cutters, lg
> monkey wrench, etc) and 13 pairs of usable tongs (5 are nice) plus
> various interesting scraps, for $70!  :))
> 
> thanks!
> 
> ~ben
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 

-- 

	-Andy V.

no .sig
go .fig


More information about the TheForge mailing list