[TheForge] 1045 Steel (?)

David E. Smucker davesmucker at hotmail.com
Tue Mar 4 13:13:13 EST 2008


HC spikes are also high in manganese, might be close to 1 percent.  30 
points of carbon is correct.  They will heat treat.

Dave Smucker
----- Original Message ----- 
From: "Ron Childers" <munlaw2 at hcsmail.com>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Tuesday, March 04, 2008 12:17 PM
Subject: RE: [TheForge] 1045 Steel (?)


> Dan,
>
> I drew a spike out to abt 1/4" x 1" and quenched in water @ a red heat. 
> Put
> it in the vice and hit it with a hammer and it snapped. I didn't think 30
> pts would do that. There must be some other alloy in the mix?
>
> Ron C
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of dan tull
> Sent: Tuesday, March 04, 2008 11:50 AM
> To: Sponsored by ABANA
> Subject: Re: [TheForge] 1045 Steel (?)
>
> Dann,
> Spec data sheet for "HC" spikes say 30 pts. carbon Max.
> Which makes them mild steel.
>
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
> 



More information about the TheForge mailing list