Pleae tell me a little more. Do you care that the file grooves are left in?
I assume you can grind the end of the file straight across the width and
then grind a little clearance or bevel so the bottom side is cutting and
curling up the metal. I assume the file is held at say 10 deg. from the
metal being worked? Is this about right?I guess you could make a 2 in in
length piece and weld or braze to a piece of metal which would be the handle
or just leave the file and use it as is ?
Thanks for your help.
Bob
----- Original Message -----
From: "Lon Humphrey" <ironcrossforge at roadrunner.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Saturday, March 01, 2008 6:42 PM
Subject: Re: [TheForge] scraper
> scraper...make it out of a old file like a hunting knife with no
> edge...thats what we use to scrape babbit bearings and fiber bearings
>
>
> ----- Original Message -----
> From: "Andrew Vida" <osan at netlabs.net>
> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Saturday, March 01, 2008 7:35 PM
> Subject: Re: [TheForge] scraper
>
>
> >A properly made scraper in the right hands can remove metal by the
> >*millionth* of an inch.
> >
> > schade at acegroup.cc wrote:
> >>
> >> On Mar 1, 2008, at 10:19 AM, Bob Smolen wrote:
> >>
> >>> Is there a practial way to make a scraper to remove a few thousandts
> >>> from a
> >>> flat surface. I am tired of used abraive paper. Alternatively, where
can
> >>> such a tool be purchased?
> >>> Thanks,
> >>> Bob
> >>>
> >>> ____________
> >>
> >>
> >>
> >> http://gfish.livejournal.com/187606.html
> >>
> >> _______________________________________________
> >> Manage membership or unsubscribe at:
> >> http://mailman.qth.net/mailman/listinfo/theforge
> >> theforge mail list group photo site is
> >> http://www.photoaccess.com
> >> Login: blacksmithblacksmith at hotmail.com
> >> password: anvil
> >> ___________
> >>
> >>
> >
> > --
> >
> > -Andy V.
> >
> > no .sig
> > go .fig
> > _______________________________________________
> > Manage membership or unsubscribe at:
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: blacksmithblacksmith at hotmail.com
> > password: anvil
> > ___________
> >
> >
> >
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
>
> --
> No virus found in this incoming message.
> Checked by AVG Free Edition.
> Version: 7.5.516 / Virus Database: 269.21.2/1305 - Release Date: 2/29/2008
6:32 PM
>
>
More information about the TheForge
mailing list